Helicity resolved Raman spectroscopy of mono- and a few-layers thick PtSe
arXiv:2310.17206 · doi:10.35848/1882-0786/acd35f
Abstract
We studied helicity resolved Raman scattering in PtSe flakes with different thicknesses. The peak amplitude of helicity-switched Raman scattering is significantly larger than that of helicity-conserved scattering for the in-plane mode, consistent with the Raman tensor analyses and conservation law of angular momentum. The peak amplitude of the helicity-switched mode is larger for the thinner flakes. In addition, we find Raman peaks near the energy levels of infrared (IR)-active and modes, only for monolayer and a few-layers thick flakes. Interestingly, these peaks manifest themselves only for helicity-switched Raman scattering; they are nearly absent for helicity-conserved scattering.
References in corpus (7)
- The Raman Fingerprint of Graphene
- Spin Transfer Torques
- Spin Seebeck insulator
- Helicity resolved Raman scattering of MoS2, MoSe2, WS2 and WSe2 atomic layers
- Type-II Dirac fermions in the PtSe class of transition metal dichalcogenides
- Truly chiral phonons in α-HgS
- Lattice dynamics and phase transitions in FeGeTe