Abstract
Here we demonstrate the controlled growth of Bi(110) and Bi(111) films on an (insulating) -AlO(0001) substrate by surface X-ray diffraction and X-ray reflectivity using synchrotron radiation. At temperatures as low as 40 K, unanticipated pseudo-cubic Bi(110) films are grown having a thickness ranging from a few to tens of nanometers. The roughness at the film-vacuum as well as at the film-substrate interface, can be reduced by mild heating, where a crystallographic orientation transition of Bi(110) towards Bi(111) is observed at 400 K. From 450 K onwards high quality and ultrasmooth Bi(111) films are formed. Growth around the transition temperature results in the growth of competing Bi(110) and Bi(111) thin film domains.
References in corpus (10)
- Topological Insulator Materials
- One-dimensional Topological Edge States of Bismuth Bilayers
- Stable nontrivial Z2 topology in ultrathin Bi (111) films: a first-principles study
- Angle Dependent Van Hove Singularities in Slightly Twisted Graphene Bilayer
- Nonlinear optical probe of tunable surface electrons on a topological insulator
- Bi(111) thin film with insulating interior but metallic surfaces
- Topologically protected quantum transport in locally exfoliated bismuth at room temperature
- Electronic phase transitions of bismuth under strain from relativistic self-consistent GW calculations
- Topologically Nontrivial Bismuth(111) Thin Films Grown on Bi2Te3
- Engineering electronic structure of a 2D topological insulator Bi(111) bilayer on Sb nanofilms by quantum confinement effect
Cited by in corpus (4)
- Single-Crystalline Metallic Films Induced by van der Waals Epitaxy on Black Phosphorus
- Evidence of directional structural superlubricity and Lévy flights in a van der Waals heterostructure
- Kinetics and the crystallographic structure of bismuth during liquefaction and solidification on the insulating substrate
- Studying Pulsed Laser Deposition conditions for Ni/C-based multi-layers