Mott transition from a diluted exciton gas to a dense electron-hole plasma in a single V-shaped quantum wire
arXiv:cond-mat/0301229 · doi:10.1103/PhysRevB.67.235324
Abstract
We report on the study of many-body interactions in a single high quality V-shaped quantum wire by means of continuous and time-resolved microphotoluminescence. The transition from a weakly interacting exciton gas when the carrier density n is less than 10^5 cm^-1 (i.e. n aX < 0.1, with aX the exciton Bohr radius), to a dense electron-hole plasma (n > 10^6 cm^-1, i.e. n aX > 1) is systematically followed in the system as the carrier density is increased. We show that this transition occurs gradually : the free carriers first coexist with excitons for n aX > 0.1, then the electron-hole plasma becomes degenerate at n aX = 0.8. We also show that the non-linear effects are strongly related to the kind of disorder and localization properties in the structure especially in the low density regime.
arXiv comment5 figures
References in corpus (5)
- Many-Body Renormalization of Semiconductor Quantum Wire Excitons: Absorption, Gain, Binding, Unbinding, and Mott Transition
- New criteria for bosonic behavior of excitons
- Excitonic lasing in semiconductor quantum wires
- Many-body Effects on Excitonic Optical Properties of Photoexcited Semiconductor Quantum Wire Structures
- Role of bound pairs in the optical properties of highly excited semiconductors: a self consistent ladder approximation approach
Cited by in corpus (5)
- Nonlinear Photoluminescence Excitation Spectroscopy of Carbon Nanotubes: Exploring the Upper Density Limit of One-Dimensional Excitons
- Controlling the charge environment of single quantum dots in a photonic-crystal cavity
- Local disorder and optical properties in V-shaped quantum wires : towards one-dimensional exciton systems
- Existence of an upper limit on the density of excitons in carbon nanotubes by diffusion-limited exciton-exciton annihilation: Experiment and theory
- InAs/InP single quantum wire formation and emission at 1.5 microns