Selective metal deposition at graphene line defects by atomic layer deposition
arXiv:1410.5153 · doi:10.1038/ncomms5781
Abstract
One-dimensional defects in graphene have strong influence on its physical properties, such as electrical charge transport and mechanical strength. With enhanced chemical reactivity, such defects may also allow us to selectively functionalize the material and systematically tune the properties of graphene. Here we demonstrate the selective deposition of metal at chemical vapour deposited graphene's line defects, notably grain boundaries, by atomic layer deposition. Atomic layer deposition allows us to deposit Pt predominantly on graphene's grain boundaries, folds, and cracks due to the enhanced chemical reactivity of these line defects, which is directly confirmed by transmission electron microscopy imaging. The selective functionalization of graphene defect sites, together with the nanowire morphology of deposited Pt, yields a superior platform for sensing applications. Using Pt-graphene hybrid structures, we demonstrate high-performance hydrogen gas sensors at room temperatures and show its advantages over other evaporative Pt deposition methods, in which Pt decorates graphene surface non-selectively.
arXiv comment27 pages, 6 main figures
References in corpus (20)
- Large-Area Synthesis of High-Quality and Uniform Graphene Films on Copper Foils
- 30 inch Roll-Based Production of High-Quality Graphene Films for Flexible Transparent Electrodes
- Ultrahigh electron mobility in suspended graphene
- Detection of Individual Gas Molecules Absorbed on Graphene
- Graphene Photonics and Optoelectronics
- Quantifying defects in graphene via Raman spectroscopy at different excitation energies
- Ultrathin epitaxial graphite: 2D electron gas properties and a route toward graphene-based nanoelectronics
- Intrinsic and Extrinsic Performance Limits of Graphene Devices on SiO2
- Imaging Grains and Grain Boundaries in Single-Layer Graphene: An Atomic Patchwork Quilt
- Control and Characterization of Individual Grains and Grain Boundaries in Graphene Grown by Chemical Vapor Deposition
- Operation of Graphene Transistors at GHz Frequencies
- Electronic transport in polycrystalline graphene
- Topological Defects in Graphene: Dislocations and Grain Boundaries
- Chemical functionalization of graphene with defects
- Structure and electronic transport in graphene wrinkles
- Tunable Kondo Effect in Graphene with Defects
- Cones, pringles, and grain boundary landscapes in graphene topology
- Multiply Folded Graphene
- Quantitatively Enhanced Reliability and Uniformity of High-κ Dielectrics on Graphene Enabled by Self-Assembled Seeding Layers
- Hydrogenated grain boundaries in graphene
Cited by in corpus (6)
- Growth and applications of two-dimensional single crystals
- Towards Non-Volatile Spin Orbit Devices: Deposition of Ferroelectric Hafnia on Monolayer Graphene/Co/HM Stacks
- Chiral nanoparticle chains on inorganic nanotube templates
- Improvement of accuracy of wave-function-matching method for transport calculation
- Metallic nanolines ruled by grain boundaries in graphene: an ab initio study
- Deep Learning Segmentation of Complex Features in Atomic-Resolution Phase Contrast Transmission Electron Microscopy Images