We study the magnetoresistance of yttrium iron garnet/Pt heterostructures in which the Pt layer was grown via atomic layer deposition (ALD). Magnetotransport experiments in three orthogonal rotation planes reveal the hallmark features of spin Hall magnetoresistance. We estimate the spin transport parameters by comparing the magnitude of the magnetoresistance in samples with different Pt thicknesses. We compare the spin Hall angle and the spin diffusion length of the ALD Pt layers to the values reported for high-quality sputter-deposited Pt films. The spin diffusion length of 1.5nm agrees well with platinum thin films reported in the literature, whereas the spin Hall magnetoresistance is approximately a factor of 20 smaller compared to that of our sputter-deposited films. Our results demonstrate that ALD allows fabricating spin-Hall-active Pt films of suitable quality for use in spin transport structures. This work provides the basis to establish conformal ALD coatings for arbitrary surface geometries with spin-Hall-active metals and could lead to 3D spintronic devices in the future.

arXiv comment11 pages, 3 figures

References in corpus (12)

Cited by in corpus (2)