Ab-initio Study of the Trimethylaluminum Atomic Layer Deposition Process on Carbon Nanotubes - An Alternative Initial Step
arXiv:1706.10056 · doi:10.1116/1.4968196
Abstract
Electronic applications of carbon nanotubes (CNTs) require the deposition of dielectric films on the tubes while conserving their excellent electronic properties. In our density functional theory study we use the trimethylaluminum (TMA) atomic layer deposition (ALD) as a model process for a CNT-functionalization. Since this functionalization relies on the presence of OH-groups, the CNTs are exposed to a water or oxygen pre-treatment. We show that only CNTs with a single-vacancy defect are able to react with HO or O. Further, the defect is preferably saturated by oxygen. This leaves the CNT without the necessary hydroxyl groups for the first TMA addition. Therefore, we propose an alternative initial step after which a classical TMA ALD process can be performed on the CNT.
arXiv comment7 pages, 6 figures, 2 tables, supplemental: 2 pages, 5 figures
References in corpus (5)
- Photoluminescence from single walled carbon nanotubes: a comparison between suspended and micelle-encapsulated nanotubes
- Band gaps of primary metallic carbon nanotubes
- High-frequency performance of scaled carbon nanotube array field-effect transistors
- DFT investigations of the piezoresistive effect of carbon nanotubes for sensor application
- Empirical transport model of strained CNT transistors used for sensor applications