Dissipation processes in the insulating skyrmion compound Cu2OSeO3
arXiv:1412.0739 · doi:10.1103/PhysRevB.90.224412
Abstract
We present a detailed study of the phase diagram surrounding the skyrmion lattice (SkL) phase of Cu2OSe2O3 using high-precision magnetic ac susceptibility measurements. An extensive investigation of transition dynamics around the SkL phase using the imaginary component of the susceptibility revealed that at the conical-to-SkL transition a broad dissipation region exists with a complex frequency dependence. The analysis of the observed behavior within the SkL phase indicates a distribution of relaxation times intrinsically related to SkL. At the SkL-to-paramagnet transition a narrow first-order peak is found that exhibits a strong frequency and magnetic field dependence. Surprisingly, very similar dependence has been discovered for the first-order transition below the SkL phase, i.e. where the system enters the helical and conical state(s), indicating similar processes across the order-disorder transition.
Accepted for publication in PRB
References in corpus (4)
- Spontaneous Skyrmion Ground States in Magnetic Metals
- Long wavelength helimagnetic order and skyrmion lattice phase in Cu2OSeO3
- Fluctuation-induced first-order phase transition in Dzyaloshinskii-Moriya helimagnets
- Electric field-induced Skyrmion distortion and giant lattice rotation in the magnetoelectric insulator Cu2OSeO3
Cited by in corpus (7)
- A.C. susceptibility as a probe of low-frequency magnetic dynamics
- Symmetry breaking, slow relaxation dynamics, and topological defects at the field-induced helix reorientation in MnSi
- Complex magnetic phases enriched by charge density waves in topological semimetals GdSb_xTe_{2-x-δ}
- Weak crystallization of fluctuating skyrmion textures in MnSi
- An ac-susceptibility study of magnetic relaxation phenomena in the antiskyrmion hosting tetragonal Mn-Pt(Pd)-Sn system
- Increasing the skyrmion stability in CuOSeO by chemical substitution
- Pinning of Helimagnetic Phase Transitions in Zn-Substituted Skyrmion Host CuOSeO