Abstract
We report the discovery of superconductivity at Tc = 3.7 K in the new ternary lithium silicide Li2IrSi3. The crystal structure of Li2IrSi3 consists of IrSi6 antiprisms connected by Si triangles, giving rise to a three dimensional framework of covalent Si-Si and Si-Ir bonds. Electronic specific-heat in superconducting phase suggests that Li2IrSi3 is a BCS weak-coupling superconductor.
15 pages, 3 figures, 1 table
References in corpus (5)
- Superconductivity in diamond
- Anisotropic thermodynamic and transport properties of single crystalline (BaK)FeAs (x = 0 and 0.45)
- Specific heat of Nb_3Sn: The case for a second energy gap
- Specific heat and electronic states of superconducting boron-doped silicon carbide
- Superconductivity in Noncentrosymmetric Iridium Silicide Li2IrSi3
Cited by in corpus (6)
- New Ternary Superconducting Compound LaRu2As2: Physical Properties from DFT Calculations
- Superconductivity in the Hexagonal Ternary Phosphide ScIrP
- Characterization of the Heavy Metal Pyrochlore Lattice Superconductor CaIr2
- Ir d-band Derived Superconductivity in the Lanthanum-Iridium System LaIr3
- Kagome metals
- No superconductivity in PbCu(PO)O found in orbital and spin fluctuation exchange calculations