Abstract
The hot-electron attenuation length in Ni is measured as a function of energy across two different Schottky interfaces viz. a polycrystalline Si(111)/Au and an epitaxial Si(111)/NiSi_2 interface using ballistic electron emission microscopy (BEEM). For similarly prepared Si(111) substrates and identical Ni thickness, the BEEM transmission is found to be lower for the polycrystalline interface than for the epitaxial interface. However, in both cases, the hot-electron attenuation length in Ni is found to be the same. This is elucidated by the temperature-independent inelastic scattering, transmission probabilities across the Schottky interface, and scattering at dissimilar interfaces.
5 pages, 5 figures
Cited by in corpus (5)
- Performance analysis of Schottky-junction-based near-field thermophotovoltaic system
- Probing electron transport across a LSMO/Nb:STO heterointerface at the nanoscale
- Hot electron transport in a strongly correlated transition metal oxide
- Probing hot electron transport across an epitaxial Schottky interface of SrRuO3/Nb:SrTiO3
- Hot electron attenuation of direct and scattered carriers across an epitaxial Schottky interface