Effect of starting materials on the superconducting properties of SmFeAsO1-xFx tapes
arXiv:1201.6522 · doi:10.1088/0953-2048/25/3/035013
Abstract
SmFeAsO1-xFx tapes were prepared using three kinds of starting materials. It shows that the starting materials have an obvious effect on the impurity phases in final superconducting tapes. Compared with the other samples, the samples fabricated by SmAs, FeO, Fe2As, and SmF3 have the smallest arsenide impurity phase and voids. As a result, these samples possess much denser structure and better grain connectivity. Moreover, among the three kinds of samples fabricated in this work, this kind of sample has the highest zero-resistivity temperature ~40 K and largest critical current density ~4600 A/cm^2 in self-field at 4.2 K. This is the highest Jc values reported so far for SmFeAsO1-xFx wires and tapes.
arXiv comment15 pages, 4 figures
References in corpus (10)
- Superconductivity at 38 K in the iron arsenide (Ba1-xKx)Fe2As2
- Superconductivity at 43 K in Samarium-arsenide Oxides
- New Fe-based superconductors: properties relevant for applications
- Intergrain current flow in a randomly oriented polycrystalline SmFeAsO0.85 oxypnictide
- High transport critical current densities in textured Fe-sheathed Sr1-xKxFe2As2+Sn superconducting tapes
- Fabrication and characterization of iron pnictide wires and bulk materials through the powder-in-tube method
- Low-Temperature Rapid Synthesis and Superconductivity of Fe-Based Oxypnictide Superconductors
- Effective Ex-Situ Fabrication of F-Doped SmFeAsO Wire for High Transport Critical Current Density
- Development of Powder-in-Tube Processed Iron Pnictide Wires and Tapes
- Evidence for electromagnetic granularity in polycrystalline Sm1111 iron-pnictides with enhanced phase purity