Analysis of interdiffusion between SmFeAsO0.92F0.08 and metals for ex situ fabrication of superconducting wire
arXiv:1106.1328 · doi:10.1088/0953-2048/24/7/075024
Abstract
We demonstrate the fabrication of superconducting SmFeAsO1-xFx (Sm-1111) wires by using the ex-situ powder-in-tube technique. Sm-1111 powder and a binder composed of SmF3, samarium arsenide, and iron arsenide were used to synthesize the superconducting core. Although the F content of Sm-1111 is reduced in the process of ex-situ fabrication, the binder compensates by sufficiently supplementing the F content, thereby preventing a decrease in the superconducting transition temperature and a shrinking of the superconducting volume fraction. Thus, in the superconducting Sm-1111 wire with the binder, the transport critical current density reaches the highest value of ~4000 A/cm2 at 4.2 K.
References in corpus (11)
- Superconductivity at 38 K in the iron arsenide (Ba1-xKx)Fe2As2
- Superconductivity at 43 K in Samarium-arsenide Oxides
- The superconductivity at 18 K in LiFeAs system
- Fabrication of the iron-based superconducting wire using Fe(Se, Te)
- Superconductivity in Epitaxial Thin Films of Co-Doped SrFe2As2 with Bilayered FeAs Structures and their Magnetic Anisotropy
- Superconducting properties of SmO1-xFxFeAs wires with Tc = 52 K prepared by the powder-in-tube method
- Electronic and Magnetic Phase Diagram of a Superconductor, SmFeAsO1-xFx
- Effective Ex-Situ Fabrication of F-Doped SmFeAsO Wire for High Transport Critical Current Density
- BaFe_{1.8}Co_{0.2}As_2 thin film hybrid Josephson junctions
- DC superconducting quantum interference devices fabricated using bicrystal grain boundary junctions in Co-doped BaFe2As2 epitaxial films
- Low-temperature synthesis of SmFeAsO0.7F0.3 wires with high transport critical current density