J. Murphy, C. P. Strehlow, K. Cho +7
Temperature-dependent London penetration depth, λ(T), was measured in optimally - doped, x=0.35, as-grown (Tc≈25 K, RRR=ρ(300K)/ρ(Tc)=4.5) and annealed ($T_c \appr…