activity
20242026
most citedScale-bridging dislocation plasticity in MgO at room temperature

5 citations · 5 across the 6 of their papers we have counts for

collaborators
Showing cond-mat.mtrl-sciShow all

7 papers · 1 filter

cond-mat.mtrl-sci2026

Resolving room temperature microscale fracture and plasticity of iron oxides along the cascade of iron ore reduction via nanoindentation and microcantilever bending

Shreehard Sahu, James P. Best, Gerhard Dehm +1

Understanding the fundamental mechanical behaviour of iron oxide phases is essential for controlling attrition and fracture during iron ore reduction process, particularly in hydro…

cond-mat.mtrl-sci2026

Defect dependent dynamic nanoindentation hardness of copper up to 25 000 s-1

Hendrik Holz, Lalith Kumar Bhaskar, Tobias Brink +4

Metals exhibit an upturn in strength at strain rates of approximately 1000 s-1 - 3000 s-1, governed by rapid dislocation multiplication, interactions and storage. This phenomenon i…

cond-mat.mtrl-sci20255 cited

Scale-bridging dislocation plasticity in MgO at room temperature

Jiawen Zhang, Zhangtao Li, Yuwei Zhang +7

Dislocations in ceramics have recently gained renewed research interest, in contrast to the traditional belief that ceramics are inherently brittle. Understanding dislocation mecha…

cond-mat.mtrl-sci2024

Microscale deformation of intermetallic-Mg interface under shear loading

Anwesha Kanjilal, Shamsa Aliramaji, Deborah Neuß +4

While intermetallic (IM)-metal interfaces in metallic alloys are critical for tuning mechanical properties, they can also act as failure sites, underscoring the importance of deter…

cond-mat.mtrl-sci2024

Thermal modification of ZrCu metallic glass nanolaminates: Structure and mechanical properties

Andrea Brognara, Chanwon Jung, Cristiano Poltronieri +4

The effects of thermal treatments on metallic glass nanolaminates (NLs), with a composition of ZrCu and ZrCu and a bilayer period of 50 nm, were explore…

cond-mat.mtrl-sci2024

Nanoscale brittle-to-ductile transition of the C15 CaAl Laves phase

Anwesha Kanjilal, Ali Ahmadian, Martina Freund +4

The influence of temperature on the deformation behaviour of the C15 CaAl Laves phase, a key constituent for enhancing the mechanical properties of Mg alloys up to service temp…