4 papers
Formation of bulk ferromagnetic nanostructured Fe40Ni40P14B6 alloys by metastable liquid spinodal decomposition
Qiang Li
Nanostructured Fe40Ni40P14B6 alloys ingots of diameter 3~5 mm could be synthesised by a metastable liquid state spinodal decomposition method. The molten Fe40Ni40P14B6 alloy was pu…
Compaction of bulk amorphous Fe40Ni40P14B6 alloys
Qiang Li
The consolidations of two bulk amorphous Fe40Ni40P14B6 alloy discs are performed via hot pressing for a short time in its supercooled liquid region under a pressure of ~1.2 GPa. Wh…
Critical cooling rate for the glass formation of ferromagnetic Fe40Ni40P14B6 alloy
Qiang Li
Bulk ferromagnetic amorphous Fe-Ni-P-B alloys in rod shape were formed by a rapid solidification technique. The largest amorphous specimen prepared had a diameter of ~2.5 mm and th…
Formation of ferromagnetic bulk amorphous Fe40Ni40P14B6 alloys
Qiang Li
Ferromagnetic bulk amorphous Fe40Ni40P14B6 alloy rods with a diameter of 1.2 mm can be prepared by means of a rapid quenching technique. If a fluxing technique is also used, amorph…