Early stages of ramified growth in quasi-two-dimensional electrochemical deposition
arXiv:patt-sol/9512003 · doi:10.1103/PhysRevE.53.R5561
Abstract
I have measured the early stages of the growth of branched metal aggregates formed by electrochemical deposition in very thin layers. The growth rate of spatial Fourier modes is described qualitatively by the results of a linear stability analysis [D.P. Barkey, R.H. Muller, and C.W. Tobias, J. Electrochem. Soc. {\bf 136}, 2207 (1989)]. The maximum growth rate is proportional to where is the current through the electrochemical cell, the electrolyte concentration, and . Differences between my results and the theoretical predictions suggest that electroconvection in the electrolyte has a large influence on the instability leading to ramified growth.
arXiv commentREVTeX, four ps figures
Cited by in corpus (5)
- Unified moving boundary model with fluctuations for unstable diffusive growth
- Kinetic roughening in a realistic model of non-conserved interface growth
- Crossover from compact to branched films in electrodeposition with surface diffusion
- Experimental investigation of the initial regime in fingering electrodeposition: dispersion relation and velocity measurements
- Anomalous Roughening of Curvature-Driven Growth With a Variable Interface Window