Neutron-diffraction study of the evolution of antiferromagnetic order in UPt3 doped with Pd
arXiv:cond-mat/9903328 · doi:10.1103/PhysRevB.60.6668
Abstract
Neutron-diffraction experiments have been carried out on U(Pt1-xPdx)3 single crystals (x<= 0.05). The small-moment antiferromagnetic order (SMAF) reported for pure UPt3 is robust upon doping and persists till at least x= 0.005. The ordered moment grows from 0.018(2) mB/U-atom for pure UPt3 to 0.048(8) mB/U-atom for x= 0.005. The Neel temperature, TN, is approximately 6 K and does not vary with Pd contents. The order parameter for the SMAF has an unusual quasi-linear temperature variation. For x>= 0.01 a large moment antiferromagnetic phase (LMAF) is found. For this phase at optimum doping (x= 0.05) TN attains a maximum value of 5.8 K and the ordered moment equals 0.63(5) mB/U-atom. TN(x) for the LMAF follows a Doniach-type phase diagram. We infer that the antiferromagnetic instability in U(Pt1-xPdx)3 is located in the range 0.5-1 at.% Pd.
arXiv comment21 pages text (PS), 6 pages with 11 Figs. (PS), submitted to Phys.Rev.B
References in corpus (5)
- The Order Parameter for the Superconducting Phases of UPt
- Absence of zero field muon spin relaxation induced by superconductivity in the B phase of UPt
- Influence of a magnetic field on the antiferromagnetic order in UPt_3
- Studies of superconductivity in U(Pt1-xPdx)3 for x < 0.006
- Suppression of Superconductivity in Single Crystals of UPt_3 by Pd Substitution
Cited by in corpus (7)
- Magnetic quantum critical point and superconductivity in UPt3 doped with Pd
- Magnetism in heavy-fermion U(Pt,Pd)3 studied by mSR
- Superconductivity in heavy-fermion U(Pt,Pd)3 and its interplay with magnetism
- Magnetic Field Effects on Neutron Diffraction in the Antiferromagnetic Phase of
- Onset of antiferromagnetism in UPt_{3} via Th-substitution studied by muon spin spectroscopy
- Muon localization site in U(Pt,Pd)3
- Antiferromagnetic Domains and Superconductivity in UPt3