Unconventional Charge Ordering in Na0.70CoO2 below 300 K
arXiv:cond-mat/0308383 · doi:10.1103/PhysRevB.69.100404
Abstract
We present the results of measurements of the dc-magnetic susceptibility chi(T) and the 23Na-NMR response of Na_{0.70}CoO_{2} at temperatures between 50 and 340 K. The chi(T) data suggest that for T > 75 K, the Co ions adopt an effective configuration of Co^{3.4+}. The 23Na-NMR response reveals pronounced anomalies near 250 and 295 K, but no evidence for magnetic phase transitions is found in chi(T). Our data suggest the onset of a dramatic change in the Co 3d-electron spin dynamics at 295 K. This process is completed at 230 K. Our results maybe interpreted as evidence for either a tendency to electron localization or an unconventional charge-density wave phenomenon within the cobalt oxide layer, CoO_2, 3d electron system near room temperature.
4 pages, 4 figures, re-submitted to Physical Review Letters. The manuscript has been revised following the recommendations of the referees. The discussion section contains substantial changes
References in corpus (7)
- Spin entropy as the likely source of enhanced thermopower in $\rm\bf Na_xCo_2O_4
- Unconventional magnetic transition and transport behavior in Na0.75CoO2
- Unconventional Superconductivity and Electron Correlations in Cobalt Oxyhydrate NaCoOHO
- Quantum Critical Behavior and Possible Triplet Superconductivity in Electron Doped CoO2 Sheets
- Crystal Structure of the Sodium Cobaltate Deuterate Superconductor NaxCoO2o4xD2O (x=1/3)
- Static magnetic order in NaCoO detected by muon spin rotation and relaxation
- 59Co-NMR Knight Shift of the Superconducting NaxCoO2.yH2O
Cited by in corpus (32)
- Magnetic ordering and spin waves in
- Crystal Structure and Elementary Properties of NaxCoO2 (x = 0.32, 0.5, 0.6, 0.75, and 0.92) in the Three-Layer NaCoO2 Family
- Possible effects of charge frustration in NaCoO: bandwidth suppression, charge orders and resurrected RVB superconductivity
- The crystal growth and characterization of NaxCoO2 and NaxCoO2yH2O
- Charge ordering and magneto-polarons in NaCoO
- 1D to 2D Na Ion Diffusion Inherently Linked to Structural Transitions in NaCoO
- NMR study of the magnetic and metal-insulator transitions in Na0.5CoO2: a nesting scenario
- Infrared spectroscopy of the charge ordering transition in NaCoO
- Bulk Electronic structure of NaCoO.1.3HO
- Structural Phase Transitions and Sodium Ordering in Na0.5CoO2: a Combined Electron Diffraction and Raman Spectroscopy Study
- Anisotropic quasiparticle renormalization in Na0.73CoO2: role of inter-orbital interactions and magnetic correlations
- Melting of the Na layers in solid Na0.8CoO2
- Magnetic properties of spin-orbital polarons in lightly doped cobaltates
- Mesoscopic phase separation in NaCoO ()
- Synthesis, Characterization, and Magnetic Properties of gamma-NaxCoO2 (0.70 < x <0.84)
- A unified origin for the 3D magnetism and superconductivity in NaCoO
- Magnetic Fluctuations in the Metallic State of NaCoO Revealed by Na NMR
- Stripe correlations in NaCoO
- Na order and Co charge disproportionation in NaCoO
- Finite temperature properties of the triangular lattice t-J model, applications to NaCoO
- 23Na NMR study of sodium order in NaxCoO2 with 22K Neel temperature
- Localized versus itinerant magnetic moments in Na0.72CoO2
- The role of the water molecules in novel superconductor, NaCoO1.3HO
- NaxCoO2: Enhanced low-energy excitations of electrons on a 2D triangular lattice
- Magnetic Phase Transition at 88 K in Na0.5CoO2 revealed by 23Na-NMR investigations
- Interplay between mesoscopic phase separation and bulk magnetism in the layered NaxCoO2
- 59Co, 23Na, and 1H NMR Studies of Double-Layer Hydrated Superconductors NaxCoO2-yH2O
- Pressure Induced Superconductivity in the New Compound ScZrCo1-
- 23Na NMR study of non-superconducting double-layer hydrate NaxCoO2.yH2O
- Na NMR Study of Layered Superconductor
- Effective Interaction between the inter-penetrating Kagome lattices in Na_xCoO_2
- Temperature-driven sodium-ion dynamical-to-static crossover in the zig-zag ordered phase of NaCoO