Abstract
We report on the synthesis of high quality LaSrFeO (LSFO) thin films using the pulsed laser deposition technique on both SrTiO (STO) and LaAlO (LAO) substrates (100)-oriented. From X-Ray diffraction (XRD) studies, we find that the films have an out-of-plane lattice parameter around 0.3865nm, almost independent of the substrate (i.e. the nature of the strains). The transport properties reveal that, while LSFO films deposited on STO exhibit an anomaly in the resistivity vs temperature at 180K (corresponding to the charge-ordered transition and associated with a transition from a paramagnetic to an antiferromagnetic state), the films grown on LAO display a very small magnetoresistance behavior and present an hysteresis around 270K under the application of a 4T magnetic field. The changes in transport properties between both substrates are discussed and compared with the corresponding single crystals.
arXiv comment9 pages, 4 figures
References in corpus (4)
- Effects of annealing and strain on La_{1-x}Ca_{x}MnO_{3} thin films: a new phase diagram in the ferromagnetic region
- Spectacular decrease of the melting magnetic field in the charge-ordered state of tensile Pr0.5Ca0.5MnO3 films
- The effect of substrate induced strain on the charge-ordering transition in Nd_{0.5}Sr_{0.5}MnO_{3} thin films
- Charge and spin ordering in Nd{1/3}Sr{2/3}FeO{3}