First Results From Nanoindentation of Vapor Diffused Nb3Sn Films on Nb
arXiv:2307.08757
Abstract
The mechanical vulnerability of the Nb3Sn-coated cavities is identified as one of the significant technical hurdles toward deploying them in practical accelerator applications in the not-so-distant future. It is crucial to characterize the material's mechanical properties in ways to address such vulnerability. Nanoindentation is a widely used technique for measuring the mechanical properties of thin films that involves indenting the film with a small diamond tip and measuring the force-displacement response to calculate the film's elastic modulus, hardness, and other mechanical properties. The nanoindentation analysis was performed on multiple vapor-diffused Nb3Sn samples coated at Jefferson Lab and Fermilab coating facilities for the first time. This contribution will discuss the first results obtained from the nanoindentation of Nb3Sn-coated Nb samples prepared via the Sn vapor diffusion technique.
21st Intl Conf Radio Frequency Superconductivity (SRF 2023)