paper

Bullseye focusing of cylindrical waves at a liquid-solid interface

arXiv:2209.11756 · doi:10.1063/5.0127709

Abstract

Two converging and superimposing shock and Rayleigh waves are generated on a glass substrate by focusing laser pulses on two concentric rings in a bullseye configuration (67\mm~and 96\mm~radii). We study experimentally the threshold for substrate damage as a function of the number of repetitions and the delay (0-20\,ns). The bullseye focusing experiments are compared to a single focusing ring. Additionally, fluid-structure interaction simulations using a Volume-of-Fluid framework are utilized to estimate the stresses. The lowest number of repetitions to attain surface damage is found for constructive superposition of the Rayleigh waves, i.e., here for a delay of ns. The observed damage is consistent with the simulations where the largest positive stresses (GPa) are achieved for bullseye focusing with \dt = 10\,ns, followed by \dt= 20\,ns which corresponds to simultaneous shock wave focusing. In all these cases, the positive stresses are followed (a few nanoseconds later) by negative stresses that can reach GPa.

References in corpus (3)