GHz Dielectric Measurement of Powdery TiO
arXiv:1904.08765
Abstract
This study experimentally determines the dielectric properties of a powdery titanium (II) oxide (TiO) material within the microwave range (0.1-13.5 GHz). The properties were determined using a coaxial airline method using a TiO/paraffin mixture at several loading fractions. A permittivity of 60 for volume fraction below 30% and 100 for volume fraction above were measured.