Single-Crystal Growth and Thermoelectric Properties of Ge(Bi,Sb)4Te7
arXiv:1301.3030 · doi:10.1088/0953-8984/25/7/075804
Abstract
The thermoelectric properties between 10 and 300 K and the growth of single crystals of n-type and p-type GeBi4Te7, GeSb4Te7, and the Ge(Bi1-xSbx)4Te7 solid solution are reported. Single crystals were grown by the modified Bridgman method, and p-type behavior was achieved by the substitution of Bi by Sb in GeBi4Te7. The thermopower in the Ge(Bi1-xSbx)4Te7 solid solution ranges from -117 muVK^-1 to +160 muVK^-1. The crossover from n-type to p-type is continuous with increasing Sb content and is observed at x = 0.15. The highest thermoelectric efficiencies among the tested n-type and p-type samples are ZnT = 0.11 and ZpT = 0.20, respectively. For an optimal n-p couple in this alloy system the composite figure of merit is ZnpT = 0.17 at room temperature.
References in corpus (4)
Cited by in corpus (4)
- Separating the bulk and surface n- to p-type transition in the topological insulator GeBi(4-x)SbxTe7
- Ultralow Thermal Conductivity and Thermoelectric Properties of Bi4GeTe7 with an Intrinsic van der Waal Heterostructure
- Multiple superconducting phases driven by pressure in the topological insulator GeSb4Te7
- Pressure-driven superconductivity in the topological insulator GeBi4Te7